Siyanür Liçiyle Altın Ekstraksiyonu

1887'de keşfedilen kimyayla cevherden altın eritme

Metallurgy & Metal Processing Global Industrial Scale $220 billion

Genel Bakış

Gold cyanidation dissolves gold from crushed ore using dilute sodium cyanide solution, a process patented by MacArthur and Forrest in 1887. Despite gold's famous chemical inertness, it dissolves readily in aerated cyanide solution due to the extraordinary stability of the gold-cyanide complex [Au(CN)₂]⁻. This process recovers over 90% of gold from ore and accounts for approximately 90% of all gold produced worldwide. Gold is recovered from the cyanide solution by adsorption onto activated carbon (CIP/CIL) or by zinc cementation (Merrill-Crowe process).

Kimyasal Süreç

Crushed and milled gold ore (typically 1-10 g Au/ton) is leached in dilute NaCN solution (0.02-0.05%) at pH 10-11 with air sparging for 24-72 hours. Gold dissolves as [Au(CN)₂]⁻. In the CIL (carbon-in-leach) process, activated carbon is added to the leach tanks to adsorb the gold complex. Loaded carbon is stripped with hot caustic cyanide, and gold is recovered by electrowinning onto steel wool cathodes, followed by smelting to dore bullion.

4Au + 8NaCN + O₂ + 2H₂O → 4Na[Au(CN)₂] + 4NaOH (Elsner equation — gold dissolution in aerated cyanide)
Au(CN)₂⁻ + C(activated) → Au(CN)₂⁻·C (carbon adsorption)
2Au(CN)₂⁻ + Zn → Zn(CN)₄²⁻ + 2Au (zinc cementation, Merrill-Crowe)

Hammaddeler

  • Sodium cyanide (NaCN) — Andrussow process (HCN from CH₄ + NH₃ + O₂) + NaOH (Gold complexing agent (lixiviant))
  • Crushed gold ore — Open pit or underground gold mining (Gold source (1-10 g/ton typical))
  • Calcium oxide (CaO, lime) — Calcination of limestone (pH control (maintains pH >10 to prevent HCN))

Son Ürünler

  • Gold dore bullion — Refined to 99.99% gold for investment, jewelry, electronics (85-95% Au, remainder Ag and base metals)
<path stroke-linecap="round" stroke-linejoin="round" d="M12 9v3.75m-9.303 3.376c-.866 1.5.217 3.374 1.948 3.374h14.71c1.73 0 2.813-1.874 1.948-3.374L13.949 3.378c-.866-1.5-3.032-1.5-3.898 0L2.697 16.126zM12 15.75h.007v.008H12v-.008z" />

Environmental Impact

Cyanide is extremely toxic to all forms of life. Tailings dam failures (Baia Mare 2000, Samarco 2015) have caused devastating environmental disasters. Cyanide-bearing tailings require detoxification (typically with H₂O₂ or SO₂/air). The International Cyanide Management Code provides voluntary standards. Mercury amalgamation by artisanal miners causes severe mercury pollution.

Güvenlik Hususları

Son İnovasyonlar

Thiosulfate leaching (non-toxic alternative) is commercially applied at Barrick's Goldstrike mine (Nevada).
Glycine-based gold leaching is being developed as a milder alternative.
Cyanide destruction using INCO SO₂/air process reduces WAD cyanide to <1 ppm in tailings.
Gold recovery from electronic waste (urban mining) uses selective leaching.

Üretim Ölçeği

3500

ton/yıl

$220 billion

Piyasa değeri

Daha fazlası Metallurgy & Metal Processing

Frequently Asked Questions

What industry uses Siyanür Liçiyle Altın Ekstraksiyonu?
Siyanür Liçiyle Altın Ekstraksiyonu is used in the metallurgy & metal processing sector at global industrial scale scale.
What process is involved in Siyanür Liçiyle Altın Ekstraksiyonu?
Crushed and milled gold ore (typically 1-10 g Au/ton) is leached in dilute NaCN solution (0.02-0.05%) at pH 10-11 with air sparging for 24-72 hours. Gold dissolves as [Au(CN)₂]⁻. In the CIL (carbon-in-leach) process, activated carbon is added to the leach tanks to adsorb the gold complex. Loaded car
What is the economic significance of Siyanür Liçiyle Altın Ekstraksiyonu?
Siyanür Liçiyle Altın Ekstraksiyonu has a market value of $220 billion and annual production of 3,500 tons.
What is the environmental impact of Siyanür Liçiyle Altın Ekstraksiyonu?
Cyanide is extremely toxic to all forms of life. Tailings dam failures (Baia Mare 2000, Samarco 2015) have caused devastating environmental disasters. Cyanide-bearing tailings require detoxification (typically with H₂O₂ or SO₂/air). The International Cyanide Management Code provides voluntary standa
What raw materials are used in Siyanür Liçiyle Altın Ekstraksiyonu?
The main raw materials include: Sodium cyanide (NaCN), Crushed gold ore, Calcium oxide (CaO, lime).